Skip to main content

HK CREATE DESIGN / FLOOR SOLUTIONS

Homes · Shops · Offices · Warehouses · Car parks

Self-levelling and floor repairsStart with a sound base.

From preparing domestic floors to refurbishing car park decks.
Identify a suitable treatment for powdering, hollow areas or uneven levels.

HK Create Design · Updated

Spreading and rolling self-levelling compound on a prepared substrate
Repair the base, level as needed, then install the finishA sound base supports the finished floor.

First identify why the floor is uneven, whether the base is sound and how the floor will be used. HK Create Design assesses local repairs, screeding, self-levelling and vehicle wearing courses separately so the quote shows which work is needed.

  • Investigate the cause of powdering, hollow areas or damp and repair the base first.
  • Check the chosen covering's flatness and moisture requirements before installation.
  • Protect drainage falls when applying levelling compound.
  • Select the levelling underlayment and the car park wearing course separately.

01 / FLOOR KNOWLEDGE

What is self-levelling? Distinguishing underlayments from finished floors

Self-levelling compounds are flowing materials that improve flatness when the substrate, primer, thickness and application are right. They are often used under timber, SPC, LVT, vinyl or carpet. Defects in the existing floor need separate assessment and repair.

Cementitious underlayment, exposed cementitious wearing screed and self-levelling epoxy are different systems. Select for the substrate, minimum and maximum thickness, moisture, finish and loads. Ordinary underlayment is unsuitable as a car park wearing course.[1]

Flatness describes surface irregularities. Level describes elevation across the floor. A fall is a deliberate slope that directs water towards a chosen outlet.

02 / READ THE FLOOR

Nine floor problems and what the photos can tell you

Visible symptoms give a starting point for inspection. Photos alone cannot establish hollow areas, the cause of cracks or slip resistance. Check the base before deciding between patch repairs, rebuilding the screed or levelling.[2][3]

Floor with loose sand and powdering

01 / Floor symptoms

Loose sand and powdering

If dust returns after sweeping, distinguish residual construction dust from a powdering screed. Remove weak material and check the damage depth and base strength. Once the base is sound, measure flatness to decide on a levelling coat.

Floor with loose, delaminated or hollow screed

02 / Floor symptoms

Loose, delaminated or hollow areas

If mortar breaks away in sections or sounds unusually hollow when tapped, map the failed areas and remove them to a sound base. A coat of levelling compound cannot re-bond detached screed beneath it.

Floor with a peeling or blistering coating

03 / Floor symptoms

Peeling or blistering old coating

Check the old coating's adhesion and identify oil contamination or moisture sources. Remove failed coatings before repairing the base. A base already within the required flatness may need no levelling coat.

Floor with potholes and chipped edges

04 / Floor symptoms

Potholes and chipped edges

Measure the depth, remove loose edges and select a repair material for the thickness and loads. If a local repair meets the requirements, one pothole need not require resurfacing the whole floor.

Floor with cracks or damaged joints

05 / Floor symptoms

Cracks or damaged joints

Determine whether the crack is moving and whether it indicates a structural problem. Crack repair and movement-joint detailing are different. Carry existing movement joints through the new system as designed. Rigid filler must not bridge them.

Floor with ponding or poor drainage

06 / Floor symptoms

Ponding or poor drainage

Check outlets for blockages, then measure levels and falls. Retain or restore the slope where drainage is required. A standard self-levelling compound will fill it level.

Floor with tyre marks and worn areas

07 / Floor symptoms

Tyre marks and wear

Black tyre marks may only be dirt. Check the wearing course where it thins or peels. Lanes, turns and ramps face different loads. Wear and slip performance depend on the entire system.

Floor with damp patches and water staining

08 / Floor symptoms

Damp and water staining

Check for leakage, moisture rising through the floor and substrate moisture content. Standard self-levelling compounds do not waterproof a floor. Moisture trapped under a finish may cause blistering and peeling.

Floor with uneven levels and steps at transitions

09 / Floor symptoms

Uneven floors and steps at transitions

Select the finish and its finished height. Survey thresholds, transitions, high and low areas. Grind high spots and patch deep lows. On a sound base, use a levelling product within its thickness range.

Does this look like your home or car park?
Take a close-up and an overall photo.

Describe your floor problem on WhatsApp

03 / FLOOR KNOWLEDGE

Choosing self-levelling compound, cement-and-sand screed or epoxy

Cement-and-sand screed can rebuild levels, make up greater thicknesses and form falls. Cementitious self-levelling compound usually improves flatness. Car park resin systems are selected for wear, slip, chemical exposure and vehicle use. A design can combine the three operations where appropriate.

“Floor repair” leaves too much open. Specify removal area, repair depth, primer, levelling, finish and movement joints to retain. Confirm compatibility across all layers, even if they share a brand.

What each of the three operations does

methodMain purposeCheck first
Cementitious self-levelling compoundImprove flatness before laying the finishSubstrate soundness, thickness, primer, moisture and floor finish
Cement-and-sand or proprietary floor screedRebuild levels, make up greater thicknesses or form fallsBonding interface, thickness, curing, falls and joints
Epoxy or PU system for vehicle trafficWear resistance, slip resistance and car park finishesTraffic, turning wear, wet-slip risk, moisture vapour and system compatibility

Use these functions to distinguish the work. The selected product and written specification govern the details. [1][5]

04 / FLOOR KNOWLEDGE

Preparing the substrate for timber, SPC and LVT flooring

Choose the floor covering first to establish substrate requirements. Add the flooring, underlay or adhesive and levelling thicknesses together. Check doors, thresholds, cabinet feet and adjoining floors. After lifting old flooring, assess adhesive residue, old mortar and loose layers.

An uneven substrate can show through thin vinyl and affect joints. Quick-Step gives different flatness limits for Alpha Vinyl and glue-down Vinyl Flex. Check the actual product specification for each SPC or timber floor.[4]

A handful of high or low spots may only need local grinding and patching. If larger areas exceed tolerance, assess full-area levelling. Measure first to avoid specifying an unnecessary coat.

Residential timber flooring and how the space is used

Homes | Timber and SPC flooring

Office floor finishes and operating conditions

Offices | Vinyl and carpet

Shop floor finishes and operating conditions

Shops | Changing floor finishes during refurbishment

Warehouse floor finishes and operating conditions

Warehouses | Specify the finish for the load

Flatness tolerances for specific flooring products

Specified flooringOver 2 metresOver 20 centimetres
Quick-Step Alpha VinylCorrect unevenness greater than 4 mmCorrect differences greater than 1 mm
Quick-Step Vinyl Flex glue-downCorrect unevenness greater than 2 mmCorrect differences greater than 0.2 mm

These are manufacturer examples for two specified products. Joint and moisture requirements also apply. Other timber or SPC products may have different tolerances. [4]

  • Remove adhesive residue and other contaminants that impair bonding
  • Measure flatness and record the method and test points
  • Check moisture and flooring installation requirements
  • Check finished heights at doors, stairs and floor transitions first

05 / FLOOR KNOWLEDGE

Self-levelling repairs and major floor defects: repair the base before the finish

If an existing levelling layer cracks, powders or delaminates, check thickness, primer, mixing water, adhesion, moisture and use. An extra coat may leave the cause unresolved. Local repair depends on the extent of the sound base and compatibility of old and new materials.

Map the extent of loose screed, remove failed material and patch or rebuild with mortar intended for floors. Cure and test it to the next layer's requirements before priming, levelling and finishing as needed. Ordinary wall render is unsuitable as a floor screed.

Repair mortars, screed bonding layers and self-levelling primers have different application conditions and drying instructions. Exposed reinforcement, slab settlement or suspected structural cracks require professional assessment first.

Compacting and striking off the floor screed
Repair or rebuild the screed to establish a sound base.
  1. 1Confirm the extent and depth of the weak layer
  2. 2Remove failed material back to a sound substrate
  3. 3Repair or replace the screed
  4. 4Cure and test to the specified criteria
  5. 5Apply self-levelling compound and finish as needed

06 / FLOOR KNOWLEDGE

Car park refurbishment: parking bays, traffic lanes and ramps

Car park floors face repeated wheel loads, turning and braking. Levelling is one part of the work. Specify wear and slip resistance, oil cleaning, markings, movement joints and drainage. Ordinary floor paint or cement underlayment alone cannot provide the full system.[5]

Covered decks, lowest basement levels, exposed decks and ramps need different systems. Assess vapour below ground and weather and waterproofing outdoors. Keep the gradient and drainage on ramps and specify a suitable slip-resistant texture. A product's compressive strength does not establish the slab's load capacity.

In an operating car park, coordinate phased closures, vehicle entrances, pedestrian routes, noisy-work hours, fire safety and management requirements. Vehicle access may need longer than foot traffic. Agree reopening against the complete system and site conditions.

Surface finishes and markings for car park bays and traffic lanes
Plan parking bays, traffic lanes, markings and joints together.
  • Bays and lanes: select the finish for traffic volume, turning wear and cleaning
  • Ramps: retain drainage falls and specify slip resistance and surface texture separately
  • Basements and exposed areas: check moisture vapour, waterproofing and weather exposure first
  • Reopen by zone: agree barriers, curing and vehicle access handover

07 / THE WORK SEQUENCE

12 work stages from survey to handover

This sequence helps plan a floor project. The stages differ for domestic flooring and car park systems. A substrate already within the finish manufacturer's flatness tolerance may need no self-levelling coat.

01

Site survey

Site survey stage

Confirm the use, approximate area, storey, access and closure window. Record where defects occur and measure door clearances.

02

Testing and confirming the system

Testing and specification stage

Check substrate type, strength, adhesion, moisture and flatness. The selected material system determines the test methods and limits.

03

Phasing and protection

Phasing and protection stage

Protect door frames, fixed equipment and adjacent finishes. Arrange waste removal, barriers and safe access.

04

Mechanical surface preparation

Mechanical surface preparation stage

Remove loose mortar, adhesive residue, existing paint and oil. Grind high points and vacuum thoroughly.

05

Repairing potholes and cracks

Pothole and crack repair stage

Patch local damage first. Where the screed has failed extensively, repair or replace it and cure according to the product instructions.

06

Joints, levels and drainage falls

Joint, level and falls detailing stage

Retain movement joints. Check door transitions and drainage directions so water will not pond and doors will clear the finished floor.

07

Prime and level where needed

Spreading and rolling self-levelling compound on a prepared substrate

Choose a compatible primer and observe its overcoating conditions. Use the specified mixing water, maintain a continuous pour, control thickness and remove entrapped air.

08

Drying and reinspection

Drying and reinspection stage

Check flatness, surface condition and moisture. Walkability, readiness for a covering and full cure occur at different stages.

09

Floor covering or vehicle traffic system

Floor finish or trafficable system installation stage

Install the selected floor covering in a home. For a car park, choose the specified resin, broadcast aggregate and topcoat for the traffic.

10

Markings and edge details

Marking and edge finishing stage

Finish each bay marking, direction arrow, drainage outlet, door edge and transition between materials.

11

Curing and handover inspection

Curing and handover inspection stage

Check the specified test points, flatness, joints and appearance. Test drainage separately at outlets.

12

Reopen once the specified conditions are met

Reopening stage

Set walking, covering and vehicle reopening times using the material, thickness, temperature, humidity and measured results. Hand over maintenance instructions.

08 / FLOOR KNOWLEDGE

Products sold as self-levelling compounds have different thickness and system requirements

The Hong Kong product data give Sikafloor-357 Level a 5–50 mm range on indoor concrete and cementitious substrates. OPTIMIX SF818 is an interior self-levelling underlayment for 3–20 mm. These ranges are specific to each product.[1][6]

Specify product brands and models, primer, repair mortar, design thickness and the highest and lowest points. Deep depressions may need initial repairs. For a trafficable resin finish, confirm system compatibility, overcoating conditions and load requirements.

Follow the latest product data for water, mixing, working time and curing. Extra water can impair performance. Verify compatibility before combining primers or topcoats from different brands.

5–50 mm

357 Level application thickness

Specification for this indoor product only. Other levelling products differ.

[1]
3–20 mm

SF818 application thickness

Specified indoor underlayment: confirm the primer and subsequent finish.

[6]
HK$22 per sq ft

Standard self-levelling example

J03 has a HK$2,800 minimum. Confirm repairs and car park systems separately.

[7]
Two stages

Repair the base before covering

Assess the substrate, then decide whether it needs levelling or can receive the finish.

[2]

09 / FLOOR KNOWLEDGE

Self-levelling prices: standard levelling and additional repairs

HK Create Design's published online price for J03 self-levelling is HK$22 per sq ft with a HK$2,800 minimum. The item includes cleaning the floor, a bonding primer and self-levelling compound. B02 sand-and-cement screeding also costs HK$22 per sq ft, with a minimum of HK$1,850. The two methods suit different jobs and site conditions.[7]

These indicative rates apply to our standard items. Extensive repairs and complete car park refurbishment need a project-specific quote. Confirm strip-out, deep repairs, moisture control, waterproofing, extra thickness, trafficable finishes, markings, night work, carrying and rubble disposal individually.

Compare quotations on the same measured area, substrate preparation, product model and thickness, then compare cost and downtime. Routine cleaning and mechanical removal of a failed screed are different scopes.

Indicative standard levelling rates and minimum charges

Our work itemReference unit priceMinimum charge
J03 Level the floor with self-levelling compoundHK$22 per sq ftHK$2,800
B02 Cement-and-sand floor screedHK$22 per sq ftHK$1,850

Company online rates for 2026, checked 2026-11-17. Confirm the substrate, thickness and additional items. These rates exclude car park reinstatement packages. [7]

Worked example, for budgeting

Residential example: standard levelling over 300 sq ft

  • Standard J03 over 300 sq ft only
  • Verify the substrate and working conditions on site

300 × HK$22 = HK$6,600

Above the HK$2,800 minimum. The standard item totals HK$6,600.

Indicative standard self-levelling item: HK$6,600.

Illustrative calculation only. Excludes strip-out, deep repairs, moisture control, floor coverings and additional work.

Worked example, for budgeting

Local levelling over 80 sq ft: allow for the minimum charge

  • Standard J03 item only
  • Check whether local work and junction detailing are feasible first

80 × HK$22 = HK$1,760

Below the HK$2,800 minimum, so the minimum applies

Indicative standard item: HK$2,800.

Repair depth, handling and additional work affect the price. This example is for indoor floors and does not cover car parks.

  • Specify the actual treatment area rather than the flat's gross floor area
  • Define removal of weak layers, repairs and moisture treatment
  • Specify the brands and thicknesses of primer, levelling layer and finish
  • List exclusions, working hours and conditions for reopening

10 / OUR SITE RECORD

Wan Chai site record: documenting the substrate

These photos from our indoor works in Wan Chai show the existing base, equipment, straightedge check and application in progress. They document an indoor job rather than a car park project.

The photos have no legible measurements and cannot verify the product, thickness, curing time or acceptance. Use measured points, material records and work records at handover.

Photos from our projects

Floor works at different stages at Dandenong Mansion, Wan Chai

Existing substrate and conduits
Existing substrate and conduits
Floor after application of self-levelling compound
Floor after application of self-levelling compound

The photos show different positions and stages of one project. They are not matched before-and-after views. The glossy surface is still wet and does not establish dryness, acceptance or readiness for flooring.

Existing indoor substrate at the Wan Chai project

01 Existing substrate

Equipment on the Wan Chai site

02 Equipment on site

Floor with uneven levels and steps at transitions

03 Straightedge check

Indoor floor application in progress in Wan Chai

04 Surface during application

11 / FLOOR KNOWLEDGE

Handover checks beyond surface appearance

Agree the acceptance method before starting. For domestic floors, check the selected covering's installation requirements. For car parks, also check drainage, texture, markings and the system requirements for the intended traffic.

Record the flatness method and test points. Check moisture against the next system's requirements and confirm that joints are retained. Log and follow up cracks, holes or delamination. Car park slip resistance requires an appropriate assessment: photos or touch alone cannot establish it.

At handover, confirm dates for walking, covering or vehicle access, cleaning methods, warranty scope and follow-up contacts. The warranty term is the one agreed in the written quote for the specific system.

  • Material model, batch and actual treatment area recorded
  • Check flatness, moisture and transitions against the specification
  • Drainage falls and movement joints have been preserved
  • Reopening times, cleaning, maintenance and follow-up agreed

12 / LET’S PLAN YOUR FLOOR

What to send for a self-levelling or car park floor enquiry

Send an overall photo, close-ups of defects, doors and drainage outlets, plus the district, approximate area, use and working hours. We will review the scope and arrange an appropriate site assessment and itemised written quotation.

Online enquiries and initial estimates are free. Site measurement arrangements and eligibility follow our current website policy and booking confirmation. Photos support an initial enquiry. A site inspection establishes the actual condition.

YOUR PROJECT BRIEF

Here are a few examples,
so we can follow up.

No registration is needed. Your details are inserted into a WhatsApp message for you to review and send.

Send the message in WhatsApp for us to receive the enquiry. You can attach photos there after opening the chat.

Open WhatsApp with these details

FAQ / BEFORE YOU START

Common self-levelling questions

01Can self-levelling compound be poured over a powdering floor?

Identify what caused the powdering and how deep the weak layer extends. Remove unsound material and repair the base. Only level once the substrate meets the product's requirements.

02Is self-levelling always needed before SPC or timber flooring?

Not necessarily. Measure the substrate against the chosen flooring specification first. Grinding or patching can correct local irregularities. Consider levelling the whole area if larger sections are outside tolerance.

03How do self-levelling compounds and traditional cement-and-sand screeds differ?

Cement-and-sand screed can restore the design level or form falls. Self-levelling compound corrects flatness within a specified thickness range. Use the product specification and site conditions to determine the method.

04What thickness of self-levelling compound is appropriate?

Thickness is product-specific. Sikafloor-357 Level is specified for 5–50 mm and OPTIMIX SF818 for 3–20 mm. Measure the high and low points and select a compatible product within its own range.[1][6]

05Can vehicles drive directly on an ordinary self-levelling floor?

A standard self-levelling underlayment cannot serve as a vehicle wearing course. Design the complete system for the substrate, traffic, drainage, slip resistance and exposure. Check that the layers are compatible.

06Will self-levelling compound waterproof a damp or water-stained floor?

Ordinary self-levelling compounds do not waterproof floors. Investigate the moisture source and substrate moisture before specifying leak repairs, moisture control and a compatible finish.

07Can self-levelling compound be used on ramps, in bathrooms or near floor drains?

Confirm the drainage design and required falls first. Ordinary self-levelling compound flows flat. Choose a compatible screed or other treatment suited to the location and slope.

08How soon can people walk on it, flooring be laid or vehicles return?

The three times differ with the material, thickness, temperature, humidity, substrate and test results. A surface that is dry to the touch or walkable may still need time before covering or taking traffic.

09Can a self-levelling floor be repaired locally?

Local repairs may be possible where the surrounding base is sound and the cause has been dealt with. Choose compatible repair materials and detail the junctions. Moving or structural cracks require separate assessment.

10Does HK$22 per sq ft cover a car park refurbishment?

No. This is our indicative unit rate for a standard levelling item, subject to a minimum. Assess car park strip-out, repairs, trafficable finishes, slip resistance, markings and phased night work separately on site.[7]

11Can self-levelling compound be applied directly over existing tiles?

Check whether the old tiles are bonded, whether any sound hollow, substrate moisture and available height. Verify that both primer and compound are specified for this substrate, even if the tiles look intact.

12What should I prepare when requesting a quote?

Send the district, approximate area, current floor photos, intended floor covering or car park use, available closure window, storey and handling restrictions. We can then discuss the scope and a site assessment.

HK CREATE DESIGN

From identifying the defect
through to an agreed work method.

Send photos, the intended use and approximate area to enquire about levelling, floor repairs or car park refurbishment.

Free site measurement through 31 December 2026 for two or more work items, with no deposit. After that, the HK$500 fee is credited against an order. Online estimates and enquiries are free.

References

Technical data and our published rates

Edited by HK Create Design. The Wan Chai section documents our work. Other images illustrate defects, uses and work stages. Overseas guidance illustrates the relevant principles. Hong Kong acceptance criteria depend on the specified system.

  1. [1] Sika Hong Kong: Sikafloor-357 Level technical data and applications ↗View:2026-11-17
  2. [2] Sika Hong Kong: common screed defects and treatments ↗View:2026-11-17
  3. [3] Ceresit: preparing floor substrates and movement joints ↗View:2026-11-17
  4. [4] Quick-Step: substrate preparation for vinyl ↗View:2026-11-17
  5. [5] Sika Hong Kong: car park flooring systems ↗View:2026-11-17
  6. [6] OPTIMIX: SF818 interior self-levelling underlayment ↗View:2026-11-17
  7. [7] HK Create Design: floor levelling rates and scope ↗View:2026-11-17

Photos cannot establish the cause on site. Structural cracking, settlement, exposed reinforcement or persistent seepage need appropriate professional assessment. Confirm materials, programme and acceptance criteria in writing.

Why talk to HK Create Design?

Understand your self-levelling and floor repairs before you decide.

Start with the current condition

We check the existing base, intended flooring and proposed timing before quoting separately for repairs, levelling and the finish.

Compare the budget line by line

Use online rates and calculators as an initial reference. Confirm site conditions, exclusions and the final price in a written quotation.

View project calculators ↗

Project photos and a local showroom

Browse photos of our projects or book a meeting at our Wong Tai Sin showroom and bring your plans. The written agreement sets out acceptance and warranty terms.