01
Ceramic Tile Adhesive and Yingsha: Basic Differences
Cement-sand mortar is a mix of cement, sand and water. It is one of Hong Kong'sMasonry and tilingmost basic materials. It is used to render walls, screed floors, form bathroom drainage falls, fill hollows and lay traditional mortar-bed tiles. A thicker mortar layer beneath the tile is compressed as the tile is set level, allowing minor unevenness to be corrected.
Ceramic tile adhesive is a dry powder pre-mixed by the factory. Just add water and stir well before use. It is a thin-layer adhesive. Take weberset TF eco as an example. The manufacturer describes it as a one-component, high-strength, waterproof tile adhesive that is suitable for marble, granite, ceramic tiles and full-body tiles. It can be attached to concrete, plaster, gypsum board, brick walls and lightweight walls.[1]. Because the formula is fixed, the water content and performance of each pack are relatively stable.
The two methods are often used together. After stripping to the cement bed or concrete, form levels and falls with cement-and-sand mortar. Once the base is ready, use a thin bed of tile adhesive. A flat rendered wall can receive adhesive directly, while an uneven wall needs levelling first.
Many owners think that using tile adhesive must be "newer and better". In fact, the most important thing to consider when choosing a tile adhesive is the underlying condition and the type of tiles. The floor of old buildings often has a height difference of a few millimeters to one or two centimeters. At this time, it is not ideal to rely solely on tile adhesive to level it, because thin-layer adhesives are not designed to make up for the thickness. On the contrary, if the bottom layer is already straight, the thickness can be controlled with ceramic tile glue, the floor will rise less, and the impact on the bottom of the door and the water level will be less.
- Cement and sand for base preparation, levelling and falls
- Tile adhesive: thin layer adhesive for facing tiles
- The uneven bottom layer needs to be dealt with first
- The two are often used together
02
What does C2TE mean? Understand the grade of ceramic tile adhesive
When buying tile adhesive, you often see the words C1, C2, T, and E. According to the classification according to the European standard EN 12004, C stands for cement-based adhesive, 2 stands for reinforced, T stands for low slip and E stands for extended open time. weberset TF eco and MAPEI Keraflex both belong to the C2TE level[1][2].
The weber manufacturer's information lists its bonding strength: 1 Newton per square millimeter or more initially, after heat aging, after immersion in water and after freezing and thawing; opening time 30 minutes; adjustment time 10 minutes; slippage 0.5mm or less; VOC content less than 10 grams per liter[1]. MAPEI Keraflex states that it can be used for about 8 hours after stirring and about 30 minutes under normal temperature and humidity.[2].
Low slip means a wall tile is less likely to move down after placement. A longer open time gives the installer more time to bed and adjust the tile. MAPEI notes that direct sun, wind, heat or an absorbent base can shorten the open time to a few minutes[2].
Ask the installer for the brand and model, then check its grade and intended use against the manufacturer's technical sheet. Open time, usable pot life and mixing water differ. The cited Weber product has a pot life of about 55 minutes after mixing[1], while MAPEI Keraflex is about 8 hours[2]. The chef should control the amount of each mixing according to the characteristics of the product. It is not advisable to open too many packages at one time, and add water before drying and mixing again.
- C: Cement based
- 2: Enhanced type
- T: low slip
- E: Extend opening hours

03
The edges are suitable for tile adhesive
Tile adhesive is often more suitable for large tiles, wall tiles and wet areas. Weber's data lists use with large-format tiles and stone, on floors,wall renderingsurfaces and concrete. Plasterboard, cement board and drywall require the specified primer first.[1]. MAPEI Keraflex is also listed as being able to be attached to cement plasters, well-maintained and dry sand floors, and interior walls with solid paint.[2].
Regarding bathrooms, the Buildings Department's "Building Maintenance Manual" mentions leakage prevention. After the floor tiles are re-paved, the gaps between the tiles should be sealed with waterproof cement; the wall tiles should be fully paved with cement mortar, and all joints should also be sealed.[4]. The key point is to "pave it completely", that is, there should not be a large number of gaps at the bottom of the bricks, otherwise water will accumulate on the surface. Use tile glue and a toothed knife to press at the same time to achieve full coverage.
A cement-and-sand mortar bed can suit greater level differences, smaller tiles or traditional laying methods. A thicker bed needs more skill to place and more time to dry.
In addition, you need to be extra careful when tiling the gypsum board walls or wooden surfaces. Weber information states that gypsum board, cement board and drywall must be treated with designated primer before applying them.[1]. In wet areas, specify suitable moisture-resistant board and a compatible waterproof layer. For a tiled kitchen or bathroom partition, agree the board, primer and adhesive system before construction.
- Large bricks and wall bricks: ceramic tile adhesive is more stable
- Gypsum board and cement board: apply primer first
- Bathroom wall tiles: full coverage
- Large height difference: first leveling the sediment in Ying

04
Tooth cutter, thickness and dosage: factory instructions
There is no estimate for the amount of tile adhesive used. The manufacturer will recommend the blade size and total thickness based on the size of the tiles. The weber data sheet lists: 300×300×10mm bricks recommend a 6mm toothed cutter, 2mm glue on the back, a total thickness of 4.5mm, and a dosage of about 6.4 kg per square meter; 600×600×15mm bricks recommend an 8–10mm toothed cutter, a total thickness of 6mm, and a dosage of about 7.2kg; 1000×1000×20mm bricks recommend 10–12mm tooth cutter, same total thickness 6mm[1].
The factory dosage formula is: the dosage per square meter is equal to the total thickness (mm) multiplied by 1.25 kilograms per square meter per millimeter.[1]. That is to say, if the bottom layer is uneven, you have to rely on tile adhesive to make it thicker. The dosage and cost will increase. Moreover, the thin layer of adhesive itself is not designed to level the surface, so it is very important that the bottom layer is flat.
MAPEI also recommends applying a thin layer of adhesive on the flat edge of a toothed knife first, and then using a suitable toothed knife to apply it to the required thickness; the back of the bricks should be fully covered, and you should press hard when laying bricks.[2]. If the mixed rubber surface has peeled, you cannot save it by sprinkling water, because the water will form an anti-adhesive film, and you should scrape it again with a toothed knife.[2]. Weber also stated that it is not advisable to apply more than 1 square meter at one time and lay the tiles first.[1].
What use does usage calculation have for property owners? The main thing is to check whether the quantity of materials quoted is reasonable. For example, a 150-square-foot bathroom wall is about 14 square meters. Based on 300×300 bricks, which is about 6.4 kilograms per square meter, it will cost about 90 kilograms, or about four packages.[1]. If the number of packages written in the quotation is very different, you can ask for the reason. It may be that the bottom layer is uneven and needs to be thickened, or it may be that the number is wrong.
- Tooth picking knife according to brick size
- The bottom layer is flat and can be applied thinly first.
- No more than 1 square meter should be applied each time
- If the rubber surface becomes peeling, it needs to be scraped again. Do not spray water on it.
Example one: retiling bathroom walls and floor
Assumptions
- Hypothetical examples, not actual quotes.
- The bathroom floor is 40 square feet and the wall is 150 square feet, using 300×300 bricks.
- Waterproofing, sanitary ware and fabrics are extra.
How to calculate quantities
- A01 Strip old wall and floor tiles to the cement bed: HK$30 per sq ft × 190 = HK$5,700
- "B02" Floor leveling with drainage slope: HK$22/square foot × 40 = HK$1,850 (based on the lowest charge)
- "D01" floor tiles: HK$78/square foot × 40 = HK$3,250 (based on the minimum charge)
- "D02" wall tile front paving: HK$78/square foot × 150 = HK$11,700
- Dosage of wall tile adhesive: 150 square feet, approximately 13.9 square meters × 6.4 kg = approximately 89 kg, approximately 4 packs of 25 kg [1].
- The total project cost is HK$22,500.
Tile removal, levelling and tiling come to about HK$22,500, excluding waterproofing and tiles.
The minimum fee is charged for the floor; additional fees will be charged if it is necessary to dig into the concrete or redo waterproofing after disassembly. (see published rates)[1]
05
Large bricks and rock slabs: double-sided glue and leveling device
Bricks of 600×1200, 800×800 or even larger are popular, which require higher flatness and adhesion of the bottom layer. MAPEI information states that exterior walls and decks, bricks larger than 900 square centimeters, heavy-duty decks, and swimming pool pools should all have adhesive (double-sided adhesive) applied to the back of the bricks to ensure complete coverage.[2]. 600×600mm is already 3,600 square centimeters, far beyond this limit.
D04 large-format tiles (600×1200 or 800×800 mm) are HK$120 per sq ft, including adhesive on both surfaces, levelling clips and two-person handling. D05 extra-large tiles or sintered slabs are HK$150 per sq ft. (see published rates). This requires more labour and work than D01 straight-pattern installation for tiles of 600×600 or smaller at HK$78.
The most common problems with large bricks are "hollow" and "high and low feet". Hollow means there is a gap at the bottom of the brick, and the sound when knocked is not real; high and low feet means there is a height difference between the two bricks. The leveler can fix the height of adjacent bricks when the glue is still wet. Combined with double-sided glue, these two problems can be reduced.
Large bricks should also be arranged in advance. The larger the bricks, the more obvious the cutting position. The cutting of bricks near the doorway, wall corner and floor should be planned in advance, and the thin bricks should be placed in an inconspicuous position as much as possible. Big bricks are heavy and prone to chipping. You need to reserve manpower for going upstairs and carrying them. Old buildings do not have elevators or elevators, so transportation costs and time must be calculated.
- Larger than 900 square centimeters require double-sided tape
- Use a leveler for large bricks
- The flatness of the bottom layer is required to be higher
- Two people are required to carry it to avoid corner collapse.

06
How long does it take to dry out and caulk?
Newly tiled or sandy floors cannot be tiled immediately. Weber information states that weberset TF eco can be used at least 7 days after the plastering is completed. Before application, the surface should be moistened with clean water and the excess water should be allowed to drain away.[1]. MAPEI also recommends at least one week of maintenance per centimeter of thickness and at least 28 days of overall maintenance for the sand platform, unless particularly quick-drying materials are used.[2]. Agree the programme with the contractor and allow the required curing time before tiling.
In terms of caulking, Weber recommends using caulking agent 6 hours after laying tiles.[1]; MAPEI Keraflex states that the walls can be caulked after 4-8 hours, and the floors can be filled after 24 hours. Light walking can be done in about 24 hours, and normal use can be done in about 14 days.[2]. Therefore, the day after laying the floor tiles, try to make it as clear as possible for people walking or carrying heavy objects.
Allow grout to dry before applying a decorative joint finish. D08 decorative grouting is HK$21 per sq ft, minimum HK$1,400. (see published rates). In frequently wet areas such as kitchens and bathrooms, decorative grout can make joints easier to clean.
- Please wait at least 7 days for new batches (depending on the product)
- Floor caulking usually takes 24 hours
- Avoid laying floor tiles within 24 hours
- Allow the underlying grout to dry before applying the decorative joint finish
You can swipe left or right on your phone to view the complete table.
| Brick size (mm) | Recommended tooth cutter (mm) | Total thickness (mm) | Dosage (kg/m²) |
|---|---|---|---|
| 300×300×10 | 6 | 4.5 | 6.4 |
| 600×300×10 | 6–8 | 6 | 7.2 |
| 600×600×15 | 8–10 | 6 | 7.2 |
| 1000×1000×20 | 10–12 | 6 | 7.2 |
The data comes from weberset TF eco product data sheet and is a theoretical dosage[1]. [1]

07
Hollow bricks? Things to avoid
The Buildings Department's "Building Maintenance Manual" lists the symptoms of external wall plastering or damaged tiles: loosening, hollow sounds when hammered, cracks, surface bulges, hollow interiors and peeling; causes include aging, structural movement, poor installation skills of workers, movement caused by cold contraction and thermal expansion, damage to expansion joints or no reserved expansion joints, and water entering the gaps between the plastering or tiles and the structure.[5]. The Buildings Department also classified the decorative bricks that were separated from the wall and made a hollow sound when knocked as damaged exterior wall finishes.[6].
The same principle applies to laying bricks indoors. Common causes include insufficient adhesive coverage on the brick base, dust or loose materials on the base layer, peeling of the adhesive before application, incomplete drying of the base layer, and insufficient brick joints. Weber specifies that the bottom layer must be free of oil, rust, sawdust, paint, plastic and loose particles.[1].
The Buildings Department also mentioned that the connection between the old wall and the new mortar, and between the new veneer and the mortar, is the key to preventing the same problem from happening again. Engineers should ensure that the old wall is properly handled, and if necessary, add adhesive to the mortar or use special adhesives for facing bricks.[4].
In terms of construction schedule, if a bathroom requires removing tiles, waterproofing, leveling, laying tiles, and caulking, there will be waiting time for each step. For example, water testing is required for waterproofing, leveling must be completely dry, and caulking is required after laying tiles. If you rush the work and compress several steps to be completed in one or two days, it is easy for hollows, cracks or water seepage to appear. I would rather prepare a few more days in exchange for a more stable effect.
If you find hollow bricks after moving in, don't be too surprised. A small amount of hollows in a small area may not burst immediately, but if the hollows are in a frequently used location, are large in scope, or the brick surface has cracks, they should be dealt with as soon as possible, because stepping on them and applying force will cause the bricks to burst, and wet areas may also allow water to seep into the bottom of the bricks. The treatment method is usually to remove the hollow bricks, clean away the old adhesive, and then lay them again.
- The bottom layer is clean and free of loose objects
- Brick back full coverage
- Leave enough brick joints
- After paving, tap lightly with a rubber hammer to check.

08
Is it possible to lay new tiles directly on top of the old tiles?
Many property owners want to save on brick demolition costs and ask if they can "build bricks on top of bricks." Technically, some adhesive manufacturers will list that they can be used on specific old veneers, but the prerequisite is that the old bricks themselves must be solid and have no hollows, and the surface treatment must be done according to the manufacturer's requirements. If the old bricks already have hollows or cracks, laying new bricks over them will only cover up the problem.
Also consider height: stacking will raise the floor, affecting the bottom of the door, the water level of the toilet and kitchen, and the height difference with other rooms. The bathroom also involves a waterproof layer. The old waterproof layer has aged and is not suitable for overlaying.
If stripping, A01 removal of old wall or floor tiles to the cement base is HK$30 per sq ft. Add HK$10 per sq ft for tightly bonded tiles or breaking out to concrete. A02 floor tile and screed removal down to concrete is HK$52 per sq ft. (see published rates). Demolition debris must be disposed of properly. The Environmental Protection Department's public fill reception facilities charge HK$71 per tonne, with a minimum charge of 1 tonne.[7].
Local replacement may suffice for a few cracked or hollow tiles. Remove damaged tiles and adjacent loose tiles, prepare the base and relay with tile adhesive. Keep spare tiles and record the model and batch to help match future repairs.
- Old bricks should be knocked first to check for hollowness
- Pay attention to the impact of rising floors on doors and drains
- It is not recommended to overlay the old waterproofing in the bathroom due to aging.
- Dispose of tile demolition waste appropriately
Example two: replacing 400 sq ft of living room flooring with 600×1200 tiles
Assumptions
- Hypothetical examples, not actual quotes.
- The floor is 400 square feet and the height difference is less than 30mm.
- Fabric is extra.
How to calculate quantities
- A01 Strip old floor tiles to the cement bed: HK$30 per sq ft × 400 = HK$12,000
- "B02" floor leveling: HK$22/square foot × 400 = HK$8,800
- "D04" Large brick paving (double-sided adhesive, leveling device): HK$120/square foot × 400 = HK$48,000
- Tile adhesive dosage: 400 square feet, approximately 37.2 square meters × 7.2 kg = approximately 268 kg, approximately 11 packages [1].
- The total project cost is HK$68,800.
Tile removal, levelling and large-format tile installation come to about HK$68,800.
Excludes rubble removal, skirting and door trimming. Level differences over 30 mm need a separate quote. (see published rates)[1]
09
The quotation must be written clearly.
When reviewing the renovation quotation, the Consumer Council pointed out that the cost of masonry work, including wall erection, bricklaying, waterproofing, plastering, tiling, stone paving, etc., generally accounts for a high proportion of the entire renovation project. It is recommended that the actual area be stated in the quotation and calculated on a per square foot basis.[3]. Masonry materials include base materials such as cement, sand and bricks, and finish materials such as tiles and stone. The Consumer Council found that most quotes excluded finishes.[3].
The Consumer Council also reminds that diagonal or herringbone shop requires higher skills from the craftsmen and may require additional charges.[3]. The published list adds 24% for diagonal or herringbone layouts. (see published rates). Have the quotation specify adhesive or cement-sand mortar, adhesive make and model, whether both surfaces are coated, tile size, levelling method, standard or decorative grout, and how far old tiles and bedding will be stripped.
The Consumer Council recommends stating the extent of floor and wall tile removal, including whether the mortar bed beneath will be hacked out. These details affect the price.[3]. Write it clearly, and there will be no arguments about "this or not" in the future.
A single tiling lump sum with no area, method or materials is hard to compare or check. Request quantities and rates for removal, levelling, waterproofing, tiling, grout and any decorative joint finish. Changes can then be costed on the same basis.
- State the area and unit price per square foot
- Indicate whether the bag contains fabric or not
- Indicate the adhesive type and model
- Write down that it should be removed to one layer on the side.

10
Public price list related to tiling
Published preparation rates include B01 cement-sand wall rendering at HK$43 per sq ft, minimum HK$2,350, and B02 screeding or floor levelling at HK$22 per sq ft, minimum HK$1,850. Level differences over 30 mm are priced separately. J03Self-levelling floorslevelling is HK$22 per sq ft, minimum HK$2,800. (see published rates).
Tiling rates per sq ft: D01 floors and D02 walls, straight-pattern tiles of 600×600 mm or smaller, HK$78, minimum HK$3,250. D03 wood-look plank tiles are HK$98, D04 large-format tiles HK$120 and D06 mosaics HK$130. (see published rates). D01 includes setting out, tile layout, laying with adhesive or adhesive mortar, grouting and finishing. D02 wall tiles are laid with tile adhesive. (see published rates).
All prices have been made public, and you can use the 117 public price calculator on the website to add or subtract items by yourself; however, the actual area, ground floor condition, and price must be confirmed on site before viewing.
Budget for strip-out, waste, levelling, waterproofing, finish tiles and grouting as well as tiling labour. In a small bathroom, removal and waterproofing can form a substantial share. Use the calculator to compare the full scope.
- Leveling: B02 or J03
- Main store: D01/D02
- Big Brick: D04
- Inclined herringbone: additional 24%
You can swipe left or right on your phone to view the complete table.
| Item | No. | Unit price | Minimum charge |
|---|---|---|---|
| Floor levelling | B02 | HK$22 per sq ft | HK$1,850 |
| Floor/wall tiles front paving | D01/D02 | HK$78 per sq ft | HK$3,250 |
| big brick | D04 | HK$120 per sq ft | HK$3,700 |
| Extra Large Brick/Slate | D05 | HK$150 per sq ft | HK$4,650 |
| Beautiful sewing | D08 | HK$21 per sq ft | HK$1,400 |
The figures are from the company's published list. Tiles are separate. The written quotation confirms the actual price. (see published rates)
11
Common mistakes are the same as owner self-examination
First, the tiles are laid before the bottom layer is dry. New plaster or new flooring has a high moisture content. Laying the tiles too early will affect the adhesion and may cause water stains on the tile surface. Second, there is too much glue on the tiles. Weber data lists about 6.3 to 7 liters of water per 25 kilogram package. The actual water consumption will be adjusted on site.[1]; Too much water will affect the strength. Third, if the area is too large to be painted at one time, the rubber surface will peel off and the tiles will be laid first.
Fourth, the large bricks do not have double-sided glue, leaving gaps at the bottom of the bricks. Fifth, there are no expansion joints or the brick joints are too narrow. The Buildings Department mentioned that cold contraction and thermal expansion and no expansion joints are one of the causes of damage to the veneer.[5]. Sixth, there are no spare bricks reserved, and the same model will not be returned for future repairs.
After laying, gently tap tiles with a rubber mallet or coin to listen for hollow areas. Lay a straightedge across adjoining tiles to check uneven edges. A small amount of water on the bathroom floor can show whether it runs to the drain. Raise issues before grouting or within the warranty period.
If it isOlder flat renovation, check for concealed pipes in the old floor. Damaging a water or drain pipe during strip-out or levelling can cause leaks. The contractor should establish pipe routes before starting, isolate water where needed and test for leaks afterwards.
- The bottom layer should be completely dry
- The amount of water is as recommended by the manufacturer.
- Large brick double-sided glue
- Reserve expansion joints and backup bricks
- After laying, tap, measure and test the water.

12
How we help choose the tiling method
HK Create Design (HK CREATE DESIGN) takes on jobs big and small, from fixing a few broken tiles and re-tiling a bathroom to large-format tiles for the whole home's floors. Our designers and tradesmen with over 15 years' experience will discuss plans with you for free and, based on your chosen tiles, substrate condition and budget, advise whether to use tile adhesive or cement-sand and whether to level first.
Send site photos to WhatsApp 5243 7747 for a free consultation or book a visit for a more accurate calculation. On-site measurement is free through 31 December 2026 for two or more work items, with no deposit. After that, the HK$500 fee is credited against the order. (see published rates). The AI quotation assistant and online calculator give initial estimates only. The written quotation after site measurement confirms the final price.
After completion, we will remove the garbage, sweep up and do basic cleaning; if deep cleaning or formaldehyde removal is required, we can have a professional cleaning company follow up.
We can also help you select the bricks together, recommend sizes and surface treatments based on space size, anti-slip needs and cleaning habits, and pre-arrange the bricks on the design drawing so that you can see the effect before starting work.
- WhatsApp 5243 7747 Free consultation
- HK$500 (rebate on order)
- AI quotation is for reference only
- Complete basic cleaning
FAQ
7 practical questions answered
01Is tile adhesive always better than cement-and-sand mortar?
No. Cement-and-sand mortar forms bases, levels floors and creates falls. Tile adhesive fixes tiles in a thin bed on a flat base. The two are often used together. C2TE adhesive generally suits large-format tiles and wall tiling[1][2].
02How thick should I apply tile adhesive?
By brick size. Weber information: The total thickness of 300×300 bricks is about 4.5mm, and the total thickness of 600×600 bricks is about 6mm. The dosage is about 6.4 to 7.2 kilograms per square meter.[1].
03When can the floor tiles be laid?
MAPEI Keraflex information: It can be used for light walking in about 24 hours. The floor will be caulked after 24 hours. It can be used normally in about 14 days.[2]; Actual according to product description.
04Do you need double-sided glue?
MAPEI recommends that bricks larger than 900 square centimeters, exterior walls and heavy-duty floors be coated with adhesive on the back to ensure complete coverage[2], reduce hollowness.
05How long does it take for a new batch of bricks to be laid?
Weber information states that it will take at least 7 days after approval[1]; MAPEI recommends that each centimeter of thickness should be maintained for about one week and that the sandy soil platform should be maintained for at least 28 days.[2].
06Is it normal that the quote does not include bricks?
A Consumer Council survey found that most contractors’ quotations did not include fabrics[3], so you need to ask clearly that the labor package includes only labor and base materials.
07How much does tiling cost per square foot?
D01 and D02 straight-pattern installation for tiles of 600×600 or smaller is HK$78 per sq ft. D04 large-format tiling is HK$120 per sq ft. (see published rates). The written quotation after site measurement confirms the final price.
CHECK THE BASIS
Data and technical basis, sources can be verified
- [1]Saint-Gobain Weber (Hong Kong): weberset TF eco product information Accessed: 2026-11-01
- [2]MAPEI: Keraflex Technical Data Sheet Accessed: 2026-11-01
- [3]Consumer Council: 12 Categories of Renovation Quotation Accessed: 2026-11-01
- [4]Buildings Department: Building Maintenance Guidebook, Chapter 4 Accessed: 2026-11-01
- [5]Buildings Department: Building Maintenance Guidebook, Chapter 3 Accessed: 2026-11-01
- [6]Buildings Department: Building deficiencies Accessed: 2026-11-01
- [7]Environmental Protection Department: Construction Waste Disposal Charging Scheme Accessed: 2026-11-01
- PricesHK Create Design 2026 detailed project budget and public price list Accessed: 2026-11-01